Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 4.38 - 7.01 kN/m | 25.0 - 40.0 pli | ASTM D624 |
Parker Chomerics CHO-SEAL 1215 Conductive Elastomer Resists highest level of EMP induced current; military gasket of choice in non-corrosive environments; excellent processing for molding and extrusion. Molded and ExtrudedRoHS Compliant Information p.. |