Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 26.3 kN/m | 150 pli | ASTM D624 |
PolyOne Versaflex™ OM 1060X-1 Thermoplastic Elastomer (TPE) Versaflex™ OM 1060X-1 is an overmolding TPE with very good adhesion to PC or ABS-based plastics. - Good Surface Aesthetics - Rubbery Feel - Soft Touch - Very Good Bond to PC, ABS, PC/ABSColor conce.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | die C; ASTM D624 |
PB1100-60 Polyurethane-based Biomedical Elastomer |
|||
Tear Strength | 26.3 kN/m | 150 pli | Machine Direction, typical properties Injection molded plaques, Die C; ASTM D412 |
Kraton® D2109 DS-W (SBS) Compound Description: Kraton D2109 DS-W is an easy processing, general purpose 45 Shore A hardness material designed for a wide variety of applications. It is supplied from North America in the physical form.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | ASTM D624 |
Multibase Multi-Flex® G 7715 TPE Styrene Ethylene Butylene Styrene Block Copolymer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Tear Strength | 26.3 kN/m | 150 pli | ASTM D624 |
Multibase Multi-Flex® TEA 4001-35 Natural TPO Thermoplastic Polyolefin Elastomer Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Tear Strength | 26.3 kN/m | 150 pli | Die B, post cured- 4 hours at 177°C; ASTM D624 |
Multibase C6-530 Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 26.3 kN/m | 150 pli | Die B |
Shin-Etsu Silicones SV-13500U Silicone Rubber SV13500U is one of a series of easy processing, general purpose silicone rubber bases. It can be used in a variety of applications requiring finishing by molding, extruding or calendaring. Product F.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Initial Tear Strength |
Saint-Gobain CHR® 2345-5 Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit .. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Initial Tear Strength |
Saint-Gobain CHR® 2975-8R Glass-Silicone Backing Silicone Adhesive Pressure Sensitive Tape Description: Silicone glass provides temperature resistance from -85°F to +500°F (-62°C to +260°C) and exceptional tensile strength and abrasion resistance. Applications include thermal .. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Initial Tear Strength |
Saint-Gobain CHR® SG16-06(R) High Performance Glass-PTFE Backing Silicone Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Initial Tear Strength |
Saint-Gobain CHR® SG23-05(R) Primary Glass-PTFE Backing Acrylic Adhesive Pressure Sensitive Tape Description: PTFE glass provide dimensional stability, high tensile strength and edge tear, operates over a temperature range from -100°F to +500°F (-73°C to 260°C), and offers better ab.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Trouser; ASTM D470 |
Lubrizol ESTANE® 58887 Ether Based Thermoplastic Polyurethane Features: Excellent hydrolysis resistance, low temperature performance, clarity and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and blow molding; cab.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR Mistron Vapor Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | ASTM D624 |
Diamond Polymers Softflex® SF 0450 Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Silicone Property; ASTM D624 |
Arlon 51586R015E 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene This data represents typical values for the production mat.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Silicone Property; ASTM D624 |
Arlon 51581R028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: Polyethylene Appearance: Red silicone gu.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Silicone Property; ASTM D624 |
Arlon 55581R028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: 162 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: PolyethyleneAppearance: Red silicone gum on.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Silicone Property; ASTM D624 |
Arlon 55589R032 0.034" (0.864 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 FiberglassAppearance: Red silicone gum and rubber on fiberglass This.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Die C; ASTM D624C-73 |
3M 8429-6 Cold Shrink Connector Insulators 3M™ Cold Shrink Connector Insulators are open-ended, tubular, rubber sleeves which are factory expanded and assembled onto a removable core. The core is removed after the tube has been positioned f.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Silicone Property; ASTM D624 |
Arlon 55580R025 0.026" (0.660 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneRubber Layer: Uncured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Red silicone gum on fiberglass clothThis data represents typical values .. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Die C; ASTM D624-73 |
3M 8461 Shield Adapter Kit 3M Shield Adapter Kits are designed to accommodate the grounding of accessories installed on conventional Tape, Longitudinally Corrugated (LC), Wire and UniShield power cables. The shield Adapter Ki.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Die C; ASTM D624C-73 |
3M EC-3 Cold Shrink End Caps 3M Cold Shrink End Caps are close-ended, tubular rubber sleeves that are factory expanded and loaded onto a removable core. When positioned over the end of a cable, or other cylindrical object the c.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® RT-3850M Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerNaturalApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceDisclaimer.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Die B; Silicone Property; ASTM D624 |
Arlon 32580R030 0.030" Uncured Silicone Rubber on PET Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberCarrier: 0.005" PETThis data represents typical values for the production material and should not be used as mate.. |
|||
Tear Strength | 26.3 kN/m | 150 pli | Silicone Property; ASTM D624 |
Arlon 47581R007 0.007" (0.178 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PESide 1: Uncured Silicone RubberSubstrate: 2113 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: PE This data represents typical values for the produc.. |