Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 45.6 kN/m | 260 pli | as molded- 10 minutes at 116°C; Die B |
Multibase SILASTIC® Q7-4765 Dow-Corning Biomedical Grade ETR Elastomer Information provided by Multibase |
|||
Tear Strength | 45.6 kN/m | 260 pli | Die B, no post cure- press cured for 5 minutes; ASTM D624 |
Multibase SILASTIC® Q7-4850 Dow-Corning Biomedical Grade Liquid Silicone Rubber Information provided by Multibase |
|||
Tear Strength | 45.6 kN/m | 260 pli | ASTM D412 |
Multibase TPSiV™ 3011-60A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Tear Strength | 45.6 kN/m | 260 pli | ASTM D412 |
Multibase TPSiV™ 3011-70A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Tear Strength | 45.6 kN/m | 260 pli | ASTM D412 |
Multibase TPSiV™ 3011-85A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Tear Strength | 45.6 kN/m | 260 pli | ASTM D412 |
Multibase TPSiV™ 3040-65A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Tear Strength | 45.6 kN/m | 260 pli | ASTM D412 |
Multibase TPSiV™ 3040-70A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Tear Strength | 45.6 kN/m | 260 pli | ASTM D412 |
Multibase TPSiV™ 3111-70A Thermoplastic Silicone Vulcanizate These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced.. |
|||
Tear Strength | 45.5 kN/m | 260 pli | ASTM D624 |
Network Polymers Softflex® 0954 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Tear Strength | 45.5 kN/m | 260 pli | ASTM D624 |
PolyOne Dynaflex™ D3204-1000-03 Thermoplastic Elastomer (TPE) Dynaflex™ D3204-1000-03 is an easy processing TPE designed for general purpose applications and is suitable for injection molding, extrusion, blow molding, and thermoforming processes. - Dry Feel -.. |
|||
Tear Strength | 45.5 kN/m | 260 pli | Die C, 510 mm/min; ASTM D624 |
PolyOne Elastamax™ EG-9182 Thermoplastic Elastomer (TPE) The Elastamax™ EG 9100 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9100 Series of compoun.. |
|||
Tear Strength | 45.5 kN/m | 260 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N650 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 45.6 kN/m | 260 pli | Die C; ASTM D624 |
Mearthane Durethaneâ„¢ S DS-265A Solid Polyurethane Elastomer TDI backbone: ester.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, .. |
|||
Tear Strength | 45.5 kN/m | 260 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR N220 (ISAF) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 45.6 kN/m | 260 pli | |
Dow Corning SILASTIC® Q7-4750 BIOMEDICAL GRADE ETR ELASTOMER, KIT Two-part, platinum-catalyzed (1:1 by weight), enhanced tear-resistant silicone elastomers are heat cured high consistency silicone rubbers designed for use by customers fabricating medical devices.I.. |
|||
Tear Strength | 45.6 kN/m | 260 pli | |
Dow Corning SILASTIC® Q7-4765 BIOMEDICAL GRADE ETR ELASTOMER, KIT Two-part, platinum-catalyzed (1:1 by weight), enhanced tear-resistant silicone elastomers are heat cured high consistency silicone rubbers designed for use by customers fabricating medical devices.I.. |
|||
Tear Strength | 45.6 kN/m | 260 pli | |
Dow Corning SILASTIC® Q7-4850 BIOMEDICAL GRADE ETR ELASTOMER, KIT Silastic® BioMedical Grade Liquid Silicone Rubbers are heat cured elastomer raw materials for use by customers fabricating medical devices.Information provided by Dow Corning |
|||
Tear Strength | 45.6 kN/m | 260 pli | ISO 34-1 |
Alliance Polymers Viprene™ G75A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G75A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tear Strength | 45.6 kN/m | 260 pli | ISO 34-1 |
Alliance Polymers Viprene™ G75A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G75A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tear Strength | 45.5 kN/m | 260 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR N220 (ISAF) Filler MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 45.5 kN/m | 260 pli | Graves |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 20 PHR N650 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
Tear Strength | 45.6 kN/m | 260 pli | 73°F; ASTM D624 |
ExxonMobil Santoprene® 8291-80TB Thermoplastic Rubber
(discontinued **) Description: A colorable thermoplastic elastomer which bonds to adhesive/epoxy spin-finished polyester or standard nylon fibers for closed-braid hose and woven-substrate products. With bonds strong.. |
|||
Tear Strength | 45.6 kN/m | 260 pli | die B; ASTM D624 |
G-2701 Styrene-based Biomedical Elastomer |