Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 20.0 - 373 kN/m | 114 - 2130 pli | Average value: 79.8 kN/m Grade Count:15 |
Overview of materials for Low Density Polyethylene (LDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Low Density Polyethylene (LDPE), Film Grade". Each property range of values reported is minimum and maxi.. |