Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 71.9 kN/m | 410 pli | Die C; ASTM D624 |
Northstar Polymers MGB-A80AQ High Performance Polyurethane Cast Elastomer System 80A This is a PTMEG/MDI base high-performance polyurethane casting system. This system is recommended to applications in which the part requires high rebound, slide abrasion, constant water contact and.. |
|||
Tear Strength | 71.8 kN/m | 410 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 6 PHR Varox DBPH-50 MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | 71.9 kN/m | 410 pli | ASTM D624 |
Huntsman IROGRAN® A 78 P 4766 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Tear Strength | 71.9 kN/m | 410 pli | 25 mil film; ASTM D624 |
Huntsman IROGRAN® A 85 P 5004 TPU-Polyether IROGRAN® A 85 P 5004 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications.Information provided by Alliance Polymers |
|||
Tear Strength | 71.9 kN/m | 410 pli | ASTM D624 |
Teknor Apex Telcar® TL-1477B AUTO UV BLACK 111 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Automotive Spec.. |
|||
Tear Strength | 71.8 kN/m | 410 pli | ASTM Die C |
TSE Industries Millathane® 5004 Millable Polyurethane Elastomer with 6 PHR Varox DBPH-50 MILLATHANE 5004 is a millable polyurethane elastomer having excellent processing characteristics. MILLATHANE 5004 stocks can be readily processed on conventional rubber equipment. Vulcanization is c.. |
|||
Tear Strength | 71.9 kN/m | 410 pli | ASTM D412 |
ACC EP RSP-AL EPI Engineered Polymers Aromatic Silicone Polyurea EP RSP-AL, Aromatic Silicone Polyurea, “Powered by Reactamine® Technology”, is a two component 100% solid Polyurea. This increases UV resistance without sacrificing physical properties. EP RSP-AL.. |
|||
Tear Strength | 71.9 kN/m | 410 pli | ASTM D412 |
ACC EP RSP EPI Engineered Polymers Silicone Polyurea EP RSP Silicone Polyurea, “Powered by Reactamine®Technology”, is a two component 100% solid Polyurea with superior performance in industrial applications. EP RSP displays extremely fast cure time.. |