Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 42.0 kN/m | 240 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 8502 LC BLK Multi-Flex® LC compounds are a new generation elastomers exhibiting improved compression set at elevated temperature. Multi-Flex® TPE compounds are based on Shell's Kraton G technology and featur.. |
|||
Tear Strength | 42.0 kN/m | 240 pli | ISO 34-1 |
PolyOne OnFlex™ S EF 80A-3S1977 Thermoplastic Elastomer (TPE) OnFlex™-S EF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver good mechanical properties together with excell.. |
|||
Tear Strength | 42.0 kN/m | 240 pli | ASTM D624 |
PolyOne Versollan™ RU 2204X Thermoplastic Elastomer (TPE) Versollan™ RU 2204X is the first of a new class of high performance, injection moldable TPU alloys developed to offer a rubbery feel and appearance, reduced cycle times, combined with the performan.. |
|||
Tear Strength | 42.0 kN/m | 240 pli | ASTM D624 |
PolyOne Dynaflex™ G2701-1000-02 Thermoplastic Elastomer (TPE) Dynaflex™ G2701-1000-02 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Adhesion to Polypropylene - Excellent Colorability - Good .. |
|||
Tear Strength | 42.0 kN/m | 240 pli | Die C, 51 mm/min; ASTM D624 |
PolyOne Geon™ Vinyl Flexible 90213 Polyvinyl Chloride, Flexible (PVC, Flexible) Provisional Product Information - Physical and Mechanical properties based on initial production.Information provided by PolyOne |
|||
Tear Strength | 42.0 kN/m | 240 pli | Die C, 2 in/min; ASTM D1004 |
PolyOne Geon™ Vinyl Flexible 90251 Polyvinyl Chloride, Flexible (PVC, Flexible) Information provided by PolyOne |
|||
Tear Strength | 42.0 kN/m | 240 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, 285ºF Cure Temperature MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 42.0 kN/m | 240 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2645 Custom Liquid Silicone Rubber - Infant Care This LSR elastomer is a specialty grade, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevated tempera.. |
|||
Tear Strength | 42.0 kN/m | 240 pli | Die B |
Momentive Performance Materials FSE7340 Heat Cured Fluorosilicone Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 42.0 kN/m | 240 pli | |
Shin-Etsu Silicones LIMSâ„¢ KE2001-40A/B Elastomer Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Tear Strength | 42.0 kN/m | 240 pli | |
Shin-Etsu Silicones LIMSâ„¢ KEG2002-60A/B Elastomer Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Tear Strength | 42.0 kN/m | 240 pli | Die C; Cross direction; ASTM D624 |
Teknor Apex Sarlink® 3170 Thermoplastic Elastomer A medium hardness, multi-purpose thermoplastic elastomer featuring excellent compression set and high temperature performance. Sarlink® 3170 can be processed by blow molding, injection molding or.. |
|||
Tear Strength | 42.0 kN/m | 240 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, 285ºF Cure Temperature MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 42.0 kN/m | 240 pli | ASTM D2240 |
UBE UBEPOL BR150 Non-Oil Extended Synthetic Rubber Vulcanizate (Cured 35 Minutes at 145°C) Description: UBEPOL BR is UBE's line of polybutadiene rubber products.Information provided by UBE. |
|||
Tear Strength | 42.0 kN/m | 240 pli | ASTM D2240 |
UBE UBEPOL VCR150 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel.. |
|||
Tear Strength | 42.0 kN/m | 240 pli | ASTM D2240 |
UBE UBEPOL VCR303 Synthetic Rubber Vulcanizate (Cured 50 Minutes at 145°C) Description: UBEPOL-VCR is a new type of synthetic rubber system developed by UBE's original technology. UBEPOL-VCR consists of micro-dispersed syndiotactic 1,2-polybutadiene (SPB) with high mel.. |
|||
Tear Strength | 42.0 kN/m | 240 pli | ASTM D624 |
ELASTO UK Dryflex® 400801S SBS Based Material, 80A Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Tear Strength | 42.0 kN/m | 240 pli | ASTM D624 |
ELASTO UK Dryflex® 402801S SBS Based Material, 80A Hardness, Black The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Tear Strength | 42.0 kN/m @Thickness 0.760 mm |
240 pli @Thickness 0.0299 in |
Split tear strength; extruded sheet; ASTM D1938 |
BASF Elastollan® 1180A10 Wire & Cable Grade Polyurethane Elastomer As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |