Mechanical Properties Metric English Comments
Tear Strength >= 7.89 kN/m
>= 45.0 pli
ASTM D624
Parker Chomerics POLASTRIP® Metal EMI Gasket
Description: POLASTRIP gasketing are composite EMI shielding and weather sealing materials. Either solid or sponge silicone may be specified as the weather seal. In POLASTRIP gasketing, EMI shieldin..
Tear Strength 7.89 kN/m
45.0 pli
ASTM D624
Parker Chomerics Tecknit Consil®-II 842 Molded Silver-Filled Silicone Elastomer
Description: CONSIL-II is a molded silicone elastomer filled with silver-coated inert particles. It provides high electrical conductivity, broadband shielding and moisture sealing. CONSIL-II is desi..
Tear Strength 7.89 kN/m
45.0 pli
TD; ISO 6383-1
Victrex® APTIV® 1000-050 Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline
APTIV PEEK 1000 series films are the unfilled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.APTI..
Tear Strength 7.89 kN/m
45.0 pli
Die B, Compound Property; ASTM D624
Arlon R36772R008 0.008" (0.203 mm) Fully Cured, Unsupported, Silicone Rubber with Fiberglass Substrate  (
Design/Construction:Side 1: Fully Cured, Unsupported, Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of, material ..
Tear Strength 7.89 kN/m
45.0 pli
Die C; ASTM D624
Mearthane Durethaneâ„¢ S DS-210A Solid Polyurethane Elastomer
TDI backbone: ester.Summary: Durethane S is a solid urethane elastomer. Formulations are individually compounded and tested to meet OEM requirements for durometer, tensile strength, tear strength, ..
Tear Strength 7.89 kN/m
45.0 pli
Initial Tear Strength
Saint-Gobain CHR® 2275-2 Extruded PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu..
Tear Strength 7.89 kN/m
45.0 pli
Initial Tear Strength
Saint-Gobain CHR® A662 Aluminum Foil Backing Acrylic Adhesive Pressure Sensitive Tape
Description: Aluminum and copper foil tapes offer high conformability, conductivity, and reflectivity at elevated temperatures. Aluminum is available with a fiberglass laminate for applications requ..
Tear Strength 7.89 kN/m
45.0 pli
Tensile Strength (Warp)
Saint-Gobain Chemfab® 2 Porous PTFE-Coated Glass
Description: Chemfab® Porous Series products are lightweight, highly porous materials commonly used as a release (non-stick) layer for composite curing, molding, and other processes that "off-gas..
Tear Strength 7.89 kN/m
45.0 pli
Initial Tear Strength
Saint-Gobain CHR® 2255-3 High Modulus PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu..
Tear Strength 7.89 kN/m
45.0 pli
Initial Tear Strength
Saint-Gobain CHR® HM650 High Modulus PTFE Film Backing Silicone Adhesive Pressure Sensitive Tape
Description: PTFE films provide a conformable release surface and exhibit a remarkably low coefficient of friction and non-stick properties. PTFE films have high temperature resistance and are virtu..
Tear Strength 7.89 kN/m
45.0 pli
Dow Corning SILASTIC® LCS-755 SILICONE RUBBER
55 Durometer, translucent, low compression set, uncatalysed Silicone Rubber Base suitable for molding.Information provided by Dow Corning
Tear Strength 7.89 kN/m
45.0 pli
Die B, Silicone Property; ASTM D624
Arlon 66211A007 0.007" (0.178 mm) Uncured Silicone Rubber Monofilament Polyester Fabric Substrate
Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Monofilament Polyester Fabric Side 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represent..
Tear Strength >= 7.89 kN/m
>= 45.0 pli
ASTM D624
Parker Chomerics POLASHEET® Metal EMI Gasket
Description: POLASHEET gasketing are composite EMI shielding and weather sealing materials. Either solid or sponge silicone may be specified as the weather seal. In POLASHEET gasketing individual mo..
Tear Strength 7.89 kN/m
45.0 pli
cured 15 mins @ 150°C
ACC QSil 553 QSI Quantum Silicones Silicone Potting Material
QSil 553 is a 100% silicone solids elastomer designed for electronic potting applications. The two-component system offers a flame retardant, thermally conductive, low modulus material that is readi..
Tear Strength 7.89 kN/m
45.0 pli
Die C (graves), 20 in/min; ASTM D624
PolyOne Synprene® RT-3810M Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:High Performance Thermoplastic ElastomerNaturalApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceDisclaimer..
Tear Strength 7.89 kN/m
45.0 pli
Die C (graves), 20 in/min; ASTM D624
PolyOne Synprene® ST-6110 Thermoplastic Elastomer - SBC  (discontinued **)
Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom..