Polymer Property : Tear Strength = 48.5 kN/m
Polymer Property :
Tear Strength =
48.5 kN/m
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Tear Strength
48.5
kN/m
277
pli
Die C, Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4725P General Purpose Molding
FormulationNordel® IP 4725P