Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 8.77 kN/m | 50.0 pli | ASTM D624 |
Parker Chomerics Tecknit NC-Consil® 750 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | ASTM D624 |
Parker Chomerics Tecknit NC-Consil® 770 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | ASTM D624 |
Parker Chomerics Tecknit NC-Consil® FR750 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | ASTM D624 |
Parker Chomerics Tecknit SC-Consil® 860 Carbon-Filled Silicone Elastomer Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Warp/Longitudinal direction |
Saint-Gobain Chemlam® RL® RL5000 PTFE-Coated Non-woven Aramid Reinforced Laminate Description: The CHEMLAM® series features unique combinations of multi-layer fluoropolymer films laminated to a variety of reinforcement fabrics. The RL product line features a film of fully sint.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M783 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M832 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Initial Tear Strength |
Saint-Gobain CHR® T903 TRIFOIL™ PTFE/Aluminum Foil Backing Silicone Adhesive Pressure Sensitive Tape Description: Aluminum and copper foil tapes offer high conformability, conductivity, and reflectivity at elevated temperatures. Aluminum is available with a fiberglass laminate for applications requ.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® 3 Porous PTFE-Coated Glass Description: Chemfab® Porous Series products are lightweight, highly porous materials commonly used as a release (non-stick) layer for composite curing, molding, and other processes that "off-gas.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® 3 Tear Resistant PTFE-Coated Glass Description: Chemfab® Tear Resistant Series is manufactured with specialized coating materials to improve tear and crease resistance. Uses for this series includes release sheets, belting and gas.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Initial Tear Strength; ASTM D624 |
Saint-Gobain COHRlastic® 300 General Purpose Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Initial Tear Strength; ASTM D624 |
Saint-Gobain COHRlastic® 9060 Wide Series General Purpose Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | ASTM D624 |
Teknor Apex UNIPRENE® 2021 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | ASTM D624 |
Teknor Apex Uniprene® UN-2012-L3 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | cured 60 mins @ 150°C |
ACC QLE 1020 QSI Quantum Silicones 45 Durometer Clear, Addition Cure Elastomer for Coating QLE 1020 is a 100% silicone solids elastomer designed for fabric or cloth coating applications. This two-component system offers a tough coating with excellent adhesion and fast cure.Key Features: .. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® RT-3820M Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerTransparentApplications:FDA (Food Contact)Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingDisclaimer: A thermoplasti.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® ST-6120 Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerTransparentOver-Molding GradeApplications:Multi-PurposeFDA (Food Contact)Market:Consumer GoodsProcessing Method:Injection MoldingPolyOne .. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M57 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |