Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 8.77 kN/m | 50.0 pli | ASTM D624 |
Parker Chomerics Tecknit NC-Consil® 750 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | ASTM D624 |
Parker Chomerics Tecknit NC-Consil® 770 Nickel Coated Graphite Filled Silicone Elastomer Description: NC-Consil is a silicone elastomer filled with Nickel coated graphite carbon particles. It provides high electrical conductivity, broadband shielding and environmental sealing. NC-Consil.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | ASTM D624 |
Parker Chomerics Tecknit SC-Consil® FR861 Carbon-Filled Silicone Elastomer Description: SC-CONSIL is a silicone elastomer filled with carbon particles. It provides superior shielding and a reliable environmental seal. The combination of carbon particles and silicone allows.. |
|||
Tear Strength | <= 8.77 kN/m | <= 50.0 pli | ASTM D624 |
Parker Chomerics CHO-SEAL® 0860 Conductive Elastomer Description: Low-end shielding and ESD protection; high tensile strength; no corrosion or fluid resistance.Extruded onlyRoHS CompliantInformation provided by Chomerics |
|||
Tear Strength | >= 8.77 kN/m | >= 50.0 pli | ASTM D624 |
Parker Chomerics METALKLIP® Clip-On EMI Gasket Description: Chomerics’ METALKLIP® gasketing is a simple, quick means of mounting on EMI gasket onto 15-20 gauge sheet metal enclosure doors or frames. EMI shielding is provided by either a carbon.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Die C; ASTM D624 |
Monmouth Rubber & Plastics Durafoamâ„¢ C45 Closed Cell Epichlorohydrin Information provided by Monmouth Rubber & Plastics Corp. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7130-1000 TPE Product Description: StarFlex P 7130-1000 is an easy processing TPE designed for injection molding. Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades ava.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Warp/Longitudinal direction |
Saint-Gobain Chemlam® RL® RL5000 PTFE-Coated Non-woven Aramid Reinforced Laminate Description: The CHEMLAM® series features unique combinations of multi-layer fluoropolymer films laminated to a variety of reinforcement fabrics. The RL product line features a film of fully sint.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarGrip GP 25-9000 TPE Product Description: StarGrip GP 25-9000 is an easy processing TPE designed for injection molding and this particular class of TPE material with excellent grip properties. Features:Soft TouchRubber.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Initial Tear Strength |
Saint-Gobain CHR® 2345-2 Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit .. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M832 Polyester Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M852 Polyester Film Backing Natural Rubber Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Initial Tear Strength |
Saint-Gobain CHR® M99 Polyester Film Backing Acrylic Adhesive Pressure Sensitive Tape Description: Polyester films have excellent dimensional stability, high tensile, tear, and impact strengths, and ultimate elongation up to 120% of its original dimensions. These films exhibit low wa.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Tensile Strength (Fill) |
Saint-Gobain Chemfab® 3 Premium PTFE-Coated Glass Description: Chemfab® Premium Series combines a superior quality glass fabric with a high level of PTFE content. Description: Chemfab® Premium is an excellent multi-purpose fabric with a smoot.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Initial Tear Strength |
Saint-Gobain CHR® K350 Polyimide Film Backing Silicone Adhesive Pressure Sensitive Tape Description: Polyimide films are employed because of their extreme heat resistance. Service temperatures range from -100°F to 500°F (-73°C to 260°C). These flame retardant films exhibit .. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Initial Tear Strength |
Saint-Gobain CHR® T603 TRIFOIL™ PTFE/Aluminum Foil Backing Acrylic Adhesive Pressure Sensitive Tape Description: Aluminum and copper foil tapes offer high conformability, conductivity, and reflectivity at elevated temperatures. Aluminum is available with a fiberglass laminate for applications requ.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Initial Tear Strength; ASTM D624 |
Saint-Gobain COHRlastic® 300 General Purpose Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | Initial Tear Strength; ASTM D624 |
Saint-Gobain COHRlastic® 9060 Wide Series General Purpose Silicone Solid Rubber Description: COHRlastic® solid silicone rubber in square sheet and continuous length form has a smooth, blemish-free surface. It is available in degrees of hardness from relatively soft 30 durome.. |
|||
Tear Strength | 8.77 kN/m | 50.0 pli | cured 60 mins @ 150°C |
ACC QLE 1020 QSI Quantum Silicones 45 Durometer Clear, Addition Cure Elastomer for Coating QLE 1020 is a 100% silicone solids elastomer designed for fabric or cloth coating applications. This two-component system offers a tough coating with excellent adhesion and fast cure.Key Features: .. |