Mechanical Properties Metric English Comments
Tear Strength 4.91 - 51.9 kN/m
28.0 - 296 pli
Average value: 17.4 kN/m Grade Count:181
Overview of materials for Silicone, Molded, Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val..