Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 4.90 - 6.86 kN/m | 28.0 - 39.2 pli | ASTM D624 |
Proto3000 Objet Digital Materials™ DM_9510 Rubber-like Prototyping Polymer Primary material: TangoGraySecondary material: TangoBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide th.. |
|||
Tear Strength | 4.90 - 6.86 kN/m | 28.0 - 39.2 pli | ASTM D624 |
Proto3000 Objet Digital Materials™ DM_9850/9750 Rubber-like Prototyping Polymer Primary material: TangoBlackPlus/TangoPlusSecondary material: VeroWhitePlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structu.. |
|||
Tear Strength | 4.91 kN/m | 28.0 pli | MD; ISO 6383-1 |
Victrex® APTIV® 1103-050M Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, 30% Mineral Filled Description: APTIV® 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance a.. |
|||
Tear Strength | 4.91 - 51.9 kN/m | 28.0 - 296 pli | Average value: 17.4 kN/m Grade Count:181 |
Overview of materials for Silicone, Molded, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Silicone, Molded, Glass Fiber Filled". Each property range of values reported is minimum and maximum val.. |
|||
Tear Strength | 4.90 kN/m | 28.0 pli | |
Momentive Performance Materials RTV31 Silicone Rubber Compound for High Temperature, Red RTV31, RTV60 and RTV88 silicone rubber compounds are high temperature two-part silicone elastomers. They are supplied ready-to-use with a base compound and DEBT (deputy tin deflagrate) as the standa.. |
|||
Tear Strength | 4.90 kN/m | 28.0 pli | |
Momentive Performance Materials RTV6702 One-Component, Modified Alkoxy Adhesive Sealant, White RTV6700 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature... |
|||
Tear Strength | 4.90 kN/m | 28.0 pli | |
Momentive Performance Materials RTV6703 One-Component, Modified Alkoxy Adhesive Sealant, Black RTV6700 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature... |
|||
Tear Strength | 4.90 kN/m | 28.0 pli | |
Momentive Performance Materials RTV6708 One-Component, Modified Alkoxy Adhesive Sealant, Translucent RTV6700 Series sealants are neutral cure, one-component, ready to use silicone adhesive sealants that cure to tough resilient silicone rubber on exposure to atmospheric moisture at room temperature... |
|||
Tear Strength | 4.91 kN/m | 28.0 pli | Die B, Silicone Property; ASTM D624 |
Arlon R38041X012 0.012" (0.305 mm) Uncured Fluorosilicone with Fiberglass Substrate Design/Construction: Interleave 1: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 2116 FiberglassSide 2: Uncured Silicone Rubber Interleave 2: Polyethylene Appearance: Gray silicone gum.. |
|||
Tear Strength | 4.91 kN/m | 28.0 pli | Die B, Fluorosilicone Property; ASTM D624 |
Arlon R37500G060 0.060" (1.52 mm) Uncured Fluorosilicone with Release PET Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Fluorosilicone Carrier: Release PETThis data represents typical values for the production material. The data should not be used to write,.. |
|||
Tear Strength | 4.91 kN/m | 28.0 pli | Die B; Silicone Property; ASTM D624 |
Arlon R37503G060 0.060" Uncured Fluorosilicone on Release PET Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured FluorosiliconeCarrier: 0.005" Release PETThis data represents typical values for the production material and should not be used .. |