Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 102 kN/m | 580 pli | ASTM D624 |
Huntsman KRYSTALFLEX® PE 501 Polyurethane Optical Aliphatic Film Key Properties:Moisture ResistanceChemical CompatibilityCooler ProcessingHigher AdhesionMultiple Design OptionNo special storage requiredInformation provided by Alliance Polymers |
|||
Tear Strength | 102 kN/m | 580 pli | Die 'C' Tear; 20 in/min; ASTM D624 |
PolyOne Elastamax XL 0233-1 Polyurethane Compound
(discontinued **) This is a static dissipative thermoplastic polyurethane compound for injection molding and extrusion applications. Physical Form: Pellet. Standard Color: Black/grey.Information provided by M. A. H.. |