Tear Strength 6.130 kN/m
34.98 pli
ASTM D624
Parker Chomerics CHO-SEAL® 6372 Graphite Filled Elastomer
EMI Gaskets. This extruded nickel-plated graphite filled elastomer addresses EMI shielding and environmental needs for both internal and external applications. It has an excellent performance in sal..