Polymer Property : Tear Strength = 6.86 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 4.90 - 6.86 kN/m
28.0 - 39.2 pli
ASTM D624
Proto3000 Objet Digital Materials™ DM_9510 Rubber-like Prototyping Polymer
Primary material: TangoGraySecondary material: TangoBlackDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structures, to provide th..
Tear Strength 4.90 - 6.86 kN/m
28.0 - 39.2 pli
ASTM D624
Proto3000 Objet Digital Materials™ DM_9850/9750 Rubber-like Prototyping Polymer
Primary material: TangoBlackPlus/TangoPlusSecondary material: VeroWhitePlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structu..