Mechanical Properties Metric English Comments
Tear Strength 12.25 kN/m
69.90 pli
ASTM D624
Parker Chomerics CHO-SEAL 1239 Conductive Elastomer
Material for waveguide choke, cover, and flange EMI shielding and pressure sealing; maximum heat transfer and minimum outgassing; hard (80 Shore A), high-strength material; available with raised lip..
Tear Strength 12.25 kN/m
69.90 pli
Parker Chomerics CHO-SEAL E6306 Conductive Elastomer
Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics
Tear Strength 12.25 kN/m
69.90 pli
ASTM D624
Parker Chomerics CHO-SEAL V6433 Conductive Elastomer
Material of choice for extensive fluid resistance; no corrosion resistance.Molded onlyRoHS CompliantInformation provided by Chomerics