Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Parker Chomerics CHO-SEAL 1239 Conductive Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone
Manufacturer Parker Chomerics
Trade Name CHO-SEAL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-SEAL 1239 Conductive Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Material for waveguide choke, cover, and flange EMI shielding and pressure sealing; maximum heat transfer and minimum outgassing; hard (80 Shore A), high-strength material; available with raised lip around iris opening for high power/high pressure applications.Molded onlyRoHS Compliant Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 4.00 - 5.50 g/cc
4.00 - 5.50 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 73 - 87
73 - 87
ASTM D2240
Tensile Strength at Break >= 4.14 MPa
>= 600 psi
ASTM D412
Elongation at Break >= 20 %
>= 20 %
ASTM D412
Tear Strength 12.25 kN/m
69.90 pli
ASTM D624
Thermal Properties Metric English Comments
Thermal Conductivity 1.90 W/m-K

@Pressure 2.07 MPa
13.2 BTU-in/hr-ft²-°F

@Pressure 300 psi
ASTM D5470
Maximum Service Temperature, Air 125 °C
257 °F
Electrical Properties Metric English Comments
Volume Resistivity 0.0070 ohm-cm
0.0070 ohm-cm
as supplied without pressure sensitive adhesive; MIL-DLT-83528
Shielding Effectiveness >= 70 dB

@Frequency 200000 Hz
>= 70 dB

@Frequency 200000 Hz
H Field; MIL-DTL-83528 Para.4.6.12
>= 110 dB

@Frequency 1.00e+8 Hz
>= 110 dB

@Frequency 1.00e+8 Hz
E Field; MIL-DTL-83528 Para.4.6.12
>= 110 dB

@Frequency 5.00e+8 Hz
>= 110 dB

@Frequency 5.00e+8 Hz
E Field; MIL-DTL-83528 Para.4.6.12
>= 110 dB

@Frequency 2.00e+9 Hz
>= 110 dB

@Frequency 2.00e+9 Hz
Plane Wave; MIL-DTL-83528 Para.4.6.12
>= 110 dB

@Frequency 1.00e+10 Hz
>= 110 dB

@Frequency 1.00e+10 Hz
Plave Wave; MIL-DTL-83528 Para.4.6.12
Descriptive Properties Value Comments
Binder Silicone & Expanded Cu Foil
EMP Survivability >0.9 kA / in
MIL-DTL-83528 Para.4.6.16
Filler Ag/Cu
Heat Aging <0.01ohm-cm
MIL-DTL-83528 Para.4.6.15
Type G
MIL-DTL-83528
Vibration Resistance, After <0.007 ohm-cm
MIL-DTL-83528 Para.4.6.13
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved