Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 12.4 kN/m | 70.8 pli | Die C/20"/min; ASTM D624 |
Network Polymers Softflex® 3300 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Tear Strength | 12.4 kN/m | 70.8 pli | Die C; ASTM D624 |
Teknor Apex Telcar® TL-1522B Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |