Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 1.48 kN/m | 8.44 pli | ISO 8067 |
Zotefoams ZOTEK® F 74 HT PVDF Foam Zotek® F 74 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and o.. |