Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 81.4 MPa @Temperature 23.9 °C |
11800 psi @Temperature 75.0 °F |
ASTM D790 |
Saint-Gobain Meldin® 7211 CM Compression Molded Graphite and PTFE Filled Polyimide Melidin® 7211 CM is a compression molded polyimide that contains 15% graphite and 10% PTFE fillers. This grade has the lowest coefficient of friction of the Meldin® 7000 series polyimides.Spe.. |