Polymer Property : Flexural Strength = 81.4 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 81.4 MPa

@Temperature 23.9 °C
11800 psi

@Temperature 75.0 °F
ASTM D790
Saint-Gobain Meldin® 7211 CM Compression Molded Graphite and PTFE Filled Polyimide
Melidin® 7211 CM is a compression molded polyimide that contains 15% graphite and 10% PTFE fillers. This grade has the lowest coefficient of friction of the Meldin® 7000 series polyimides.Spe..