Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 14.5 MPa @Temperature 288 °C |
2100 psi @Temperature 550 °F |
ASTM D790 |
Saint-Gobain Meldin® 5055 Thermoplastic Bearing Material General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin.. |