Polymer Property : Flexural Strength = 2100 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 14.5 MPa

@Temperature 288 °C
2100 psi

@Temperature 550 °F
ASTM D790
Saint-Gobain Meldin® 5055 Thermoplastic Bearing Material
General Notes on Meldin 3000/5000 Series Bearing Products:Injection Moldable, High-Performance Bearings. Can withstand environments of high temperature, corrosive, and water.Specific Notes on Meldin..