Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 150 MPa @Strain 5.00 % |
21800 psi @Strain 5.00 % |
d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® BM 240 000000 Nylon 6, Mineral Reinforced PA 6, injection molding, 40% mineral, isotopic properties, low warpageInformation provided by LANXESS. |
|||
Flexural Strength | 150 MPa @Strain 3.90 % |
21800 psi @Strain 3.90 % |
d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, halogen free flame retardant.Information provided by LANXESS. |
|||
Flexural Strength | 150 MPa @Strain 5.80 % |
21800 psi @Strain 5.80 % |
cond., 2 mm/min; ISO 178-A |
Lanxess Durethan® DP BKV 30 XF 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, improved flowability, improved surface finishInformation provided by LANXESS. |
|||
Flexural Strength | 150 MPa @Temperature 80.0 °C |
21800 psi @Temperature 176 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-402 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 150 MPa @Temperature 80.0 °C |
21800 psi @Temperature 176 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-403 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 150 MPa @Temperature 23.0 °C |
21800 psi @Temperature 73.4 °F |
ISO 178 |
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT
(Unverified Data**) Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |