Polymer Property : Flexural Strength = 18.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 18.0 MPa

@Temperature 175 °C
2610 psi

@Temperature 347 °F
ISO 178
Victrex® PEEK 450FE20 Polyetheretherketone, 20% PTFE
Product Description:High performance thermoplastic material, 20% filled with PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA foo..