Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 18.0 MPa @Temperature 175 °C |
2610 psi @Temperature 347 °F |
ISO 178 |
Victrex® PEEK 450FE20 Polyetheretherketone, 20% PTFE Product Description:High performance thermoplastic material, 20% filled with PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA foo.. |