Polymer Property : Flexural Strength = 33400 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 230 MPa

@Temperature 125 °C
33400 psi

@Temperature 257 °F
ISO 178
Victrex® PEEK 150GL30 30% Glass Fiber Reinforced
Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact c..
Flexural Strength 230 MPa

@Temperature 23.0 °C
33400 psi

@Temperature 73.4 °F
ISO 178
Victrex® PEEK 450FC30 General Purpose
Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and ext..
Flexural Strength 230 MPa

@Temperature 125 °C
33400 psi

@Temperature 257 °F
ISO 178
Victrex® PEEK 90GL30 BLACK EU 30% Glass Fiber Filled, PolyEtherEtherKetone
High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, FDA and EU food contact compliant, ..
Flexural Strength 230 MPa

@Temperature 125 °C
33400 psi

@Temperature 257 °F
ISO 178
Victrex® PEEK 90GL30 Polyetheretherketone, 30% Glass Fiber Reinforced
Product Description:High performance thermoplastic material, 30% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta..
Flexural Strength 230 MPa

@Strain 2.50 %
33400 psi

@Strain 2.50 %
d.a.m., 2 mm/min; ISO 178-A
Lanxess Durethan® BKV 25 F30 000000 Nylon 6, Glass Fiber Reinforced, Flame Retardant
PA 6, 25% glass fibers, injection molding, flame retardantInformation provided by LANXESS.
Flexural Strength 230 MPa

@Strain 5.00 %
33400 psi

@Strain 5.00 %
Conditioned; ISO 178
Lanxess Durethan® BKV 50 H3.0 000000 Nylon 6, 50% Glass Fibers
PA 6, 50% glass fibers, injection molding, heat-ageing stabilized
Flexural Strength 230 MPa

@Temperature 23.0 °C
33400 psi

@Temperature 73.4 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-602G30 MXD66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 230 MPa

@Temperature 80.0 °C
33400 psi

@Temperature 176 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® TY-592GHV 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 230 MPa

@Temperature 23.0 °C
33400 psi

@Temperature 73.4 °F
ISO 178
Victrex® PEEK 150FC30 Easy Flow
Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy ..