Mechanical Properties Metric English Comments
Flexural Strength 34.40 MPa

@Temperature 1200 °C
4989 psi

@Temperature 2192 °F
after Firing; ASTM-349
Stellar Canada CERAMITE® CSA Wear Resistant Castable