Material Notes:
Ceramite is a family of wear resistant castables with a unique combination of high wear resistance, thermal resistance and mechanical strength. Ceramite is produced and supplied to end users world wide, both as mortars and as various precast components. Ceramite can easily be mixed, cast and shaped in any size and is thus comfortably to work with in-situ. Ceramite can be used in within a wide range of temperatures and applications exposed to thermal shock conditions in industries like for example aluminum, cement and ferro.Applications: Floor Tile, Hearth/Furnace Tile, Furnace Sills & Doors, Lintels, Pipe and Duct Linings, Feed Tubes, Troughs/Launders, Ladles, Dampers, Nozzle Blasters, Crucible Linings, Vortex, Burner Tip Cooler Plates, Nose Ring, Electrical Insulation, Cold Wear AreasSpecific Notes on This Grade: A castable with extreme abrasion resistance and excellent thermo shock and alkali resistance properties. A castable which can be used in all industries where abrasion and thermo shock are problems. References from valves and lining of pipes and ducts for material transport in hot and extreme abrasive environments as well as areas in contact with molten metal.Information provided by Stellar Canada.
Physical Properties Metric English Comments
Bulk Density 2.88 g/cc
0.104 lb/in³
As Placed
Porosity 14 %
14 %
Apparent
Mechanical Properties Metric English Comments
Modulus of Rupture 0.0280 GPa
4.06 ksi
Hot, prefired at 1832°F/24 hours (1000°C)
Flexural Strength 25.3 MPa

@Temperature 850.0 °C
3670 psi

@Temperature 1562 °F
after Firing; ASTM-349
26.40 MPa

@Temperature 500 °C
3829 psi

@Temperature 932 °F
after Firing; ASTM-349
32.41 MPa

@Temperature 1000 °C
4701 psi

@Temperature 1832 °F
after Firing; ASTM-349
34.40 MPa

@Temperature 1200 °C
4989 psi

@Temperature 2192 °F
after Firing; ASTM-349
Compressive Strength 138.01 MPa
20016 psi
Cold Crushing after 1560°F
70.002 MPa

@Temperature 20.0 °C
10153 psi

@Temperature 68.0 °F
after 7 days
115.0 MPa

@Temperature 850 °C
16680 psi

@Temperature 1560 °F
after Firing; ASTM C-349
117.0 MPa

@Temperature 1200 °C
16970 psi

@Temperature 2190 °F
after Firing; ASTM C-349
139.01 MPa

@Temperature 1000 °C
20161 psi

@Temperature 1830 °F
after Firing; ASTM C-349
150.00 MPa

@Temperature 500 °C
21756 psi

@Temperature 932 °F
after Firing; ASTM C-349
Thermal Properties Metric English Comments
Thermal Conductivity 12.0 W/m-K

@Temperature 600.0 °C
83.2 BTU-in/hr-ft²-°F

@Temperature 1112 °F
13.89 W/m-K

@Temperature 300 °C
96.37 BTU-in/hr-ft²-°F

@Temperature 572 °F
Maximum Service Temperature, Air 1500 °C
2730 °F
Component Elements Properties Metric English Comments
Al2O3 12 %
12 %
CaO 1.7 %
1.7 %
Fe2O3 0.020 %
0.020 %
K2O 0.020 %
0.020 %
MgO 0.010 %
0.010 %
Na2O 0.040 %
0.040 %
SiC 75 %
75 %
SiO2 10 %
10 %
Descriptive Properties Value Comments
Application Prefired
Precast Shapes