Mechanical Properties Metric English Comments
Flexural Strength 45.0 MPa

@Temperature 275 °C
6530 psi

@Temperature 527 °F
ISO 178
Victrex® PEEK 450FC30 General Purpose
Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and ext..
Flexural Strength 45.0 MPa

@Temperature 80.0 °C
6530 psi

@Temperature 176 °F
Practical Use (Water Absorption 3.0%); ASTM-D790
Toyobo GLAMIDE® T-400G15 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 45.0 MPa

@Temperature 23.0 °C
6530 psi

@Temperature 73.4 °F
Practical Use (Water Absorption 3.0%); ASTM-D790
Toyobo GLAMIDE® T-808-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 45.0 MPa

@Temperature 80.0 °C
6530 psi

@Temperature 176 °F
Practical Use (Water Absorption 1.9%); ASTM-D790
Toyobo GLAMIDE® TY-502NZ 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 45.0 MPa

@Temperature -40.0 °C
6530 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 2.0%); ASTM-D790
Toyobo GLAMIDE® T-222SA Nylon/Elastomer
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 45.0 MPa

@Temperature 150 °C
6530 psi

@Temperature 302 °F
ISO 178
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT  (Unverified Data**)
Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis..
Flexural Strength 45.0 MPa

@Temperature 275 °C
6530 psi

@Temperature 527 °F
ISO 178
Victrex® PEEK 150FC30 Easy Flow
Product Description: High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding, easy ..
Flexural Strength 45.0 MPa

@Temperature 275 °C
6530 psi

@Temperature 527 °F
ISO 178
Victrex® PEEK 650GL30 30% Glass Fiber Filled, PolyEtherEtherKetone
High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, color natural/beige.Typical..