Flexural Strength 323 MPa

@Thickness 1.57 mm
46800 psi

@Thickness 0.0620 in
CW; ASTM D790
Industrial Laminates/Norplex NP555 Carbon Fiber  (discontinued **)
Description: NP555 is composed of carbon fiber fabric and a phenolic resin system. It has excellent moisture resistance and physical properties. This material was designed to replace asbestos vane m..