Polymer Property : Flexural Strength = 4701 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 32.41 MPa

@Temperature 1000 °C
4701 psi

@Temperature 1832 °F
after Firing; ASTM-349
Stellar Canada CERAMITE® CSA Wear Resistant Castable
Ceramite is a family of wear resistant castables with a unique combination of high wear resistance, thermal resistance and mechanical strength. Ceramite is produced and supplied to end users world w..