Polymer Property : Flexural Strength = 586 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Strength 586 MPa

@Temperature 23.9 °C
85000 psi

@Temperature 75.0 °F
Dry; ASTM D790
Park Electrochemical Nelcote® E-720 Epoxy Prepreg, 7781 E-Glass Reinforced
Nelcote® E-720 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-720 has a proven history in many demanding aerospac..
Flexural Strength 586 MPa

@Temperature 23.9 °C
85000 psi

@Temperature 75.0 °F
Dry, Autoclave with Post-Cure; ASTM D790
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 581 Quartz Reinforced
Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac..
Flexural Strength 586 MPa

@Temperature 23.9 °C
85000 psi

@Temperature 75.0 °F
Wet (2 hour water boil); ASTM D790
Park Electrochemical Nelcote® P-650R Polyester Prepreg, 7781 E-Glass Reinforced
Nelcote® P-650R is a non-styrenated/low VOC polyester resin system that has been designed for optical clarity. P-650 exhibits good mechanical properties up to 250°F.Key Features and Benefits:Non-s..
Flexural Strength 586 MPa

@Temperature 82.2 °C
85000 psi

@Temperature 180 °F
0° Direction, Wet; ASTM D790
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 581 Quartz Reinforced
Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp..
Flexural Strength 586 MPa

@Thickness 1.57 mm
85000 psi

@Thickness 0.0620 in
LW; ASTM D790
Industrial Laminates/Norplex NP130HF Glass Fabric
Description: High flexural, impact and tensile strength glass fabric epoxy laminate, especially in the machine direction. Engineered to provide better physical properties than NEMA FR-4. More dimens..
Copyright © lookpolymers.com All Rights Reserved