Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 414 MPa @Temperature 177 °C |
60000 psi @Temperature 350 °F |
Dry; ASTM D790 |
Park Electrochemical Nelcote® E-720 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-720 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-720 has a proven history in many demanding aerospac.. |
|||
Flexural Strength | 414 MPa @Temperature 71.1 °C |
60000 psi @Temperature 160 °F |
Wet; ASTM D790 |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 120 E-Glass Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Flexural Strength | 414 MPa @Thickness 1.57 mm |
60000 psi @Thickness 0.0620 in |
CW; ASTM D790 |
Industrial Laminates/Norplex NP130 Glass Fabric Description: Woven glass fabric combined with a halogenated epoxy resin system. Produced to printed circuit board quality standards. Flame retardant, meets UL-94 flammability classification V-0.Thic.. |
|||
Flexural Strength | 414 MPa @Temperature 1000 °C |
60000 psi @Temperature 1830 °F |
|
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon Engineered ceramic composite structure.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiCPhysical Attributes: Dense Matrix ( |