Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 0.001407 MPa @Shear Rate 10.0 1/s, Temperature 290 °C |
0.2041 psi @Shear Rate 10.0 1/s, Temperature 554 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 158 NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Zytel 158 NC010 is an intermediate viscosity PA 612 resin.Information provided by DuPont Performance Polymers |