Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 70.3 MPa @Temperature 90.6 °C |
10200 psi @Temperature 195 °F |
0° Short Beam, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber Information provided by HexCel |
|||
Shear Strength | 70.3 MPa @Temperature 90.6 °C |
10200 psi @Temperature 195 °F |
Fill Short Beam, Dry |
Hexcel® HexPly® 8552 Epoxy Matrix, A193-PW Fiber Information provided by HexCel |
|||
Shear Strength | 70.0 MPa @Temperature 22.0 °C |
10200 psi @Temperature 71.6 °F |
0°, IL |
Hexcel® HexPly® 954-6 Curing Cyanate Resin, M55J Fiber Information provided by HexCel |
|||
Shear Strength | 70.0 MPa @Temperature 232 °C |
10200 psi @Temperature 450 °F |
T300; In Plane; AMB |
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Fabric Form Fibers: T300-3K, AS4C-3KInformation provided by HexCel |
|||
Shear Strength | 70.0 MPa @Temperature 177 °C |
10200 psi @Temperature 351 °F |
AS4C; In Plane; Wet condition |
Hexcel® HexPly® M65 Bismaleimide Resin, Carbon Fabric Form Fibers: T300-3K, AS4C-3KInformation provided by HexCel |