Material Notes:
Information provided by HexCel
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.9 MPa

@Temperature 23.0 °C
4190 psi

@Temperature 73.4 °F
Flatwise, 0°
40.0 MPa

@Temperature 23.0 °C
5800 psi

@Temperature 73.4 °F
90°
2165 MPa

@Temperature 23.0 °C
314000 psi

@Temperature 73.4 °F
Tensile Modulus 6.20 GPa

@Temperature 23.0 °C
899 ksi

@Temperature 73.4 °F
90°
321 GPa

@Temperature 23.0 °C
46600 ksi

@Temperature 73.4 °F
Compressive Yield Strength 896 MPa

@Temperature 23.0 °C
130000 psi

@Temperature 73.4 °F
Compressive Modulus 300 GPa

@Temperature 23.0 °C
43500 ksi

@Temperature 73.4 °F
Shear Modulus 4.70 GPa

@Temperature 23.0 °C
682 ksi

@Temperature 73.4 °F
Shear Strength 70.0 MPa

@Temperature 22.0 °C
10200 psi

@Temperature 71.6 °F
0°, IL
78.0 MPa

@Temperature 23.0 °C
11300 psi

@Temperature 73.4 °F
Users viewing this material also viewed the following: