Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 124 MPa @Temperature -54.0 °C |
18000 psi @Temperature -65.2 °F |
Short Beam |
Hexcel® HexPly® F263 Epoxy Resin, T3T145 Carbon Tape Hexcel designation: T_145-12"-F263; Various fibersInformation provided by HexCel |
|||
Shear Strength | 124 MPa @Temperature 23.0 °C |
18000 psi @Temperature 73.4 °F |
In-Plane; prEN6032 |
Hexcel® HexPly® M35-4 80-180°C Curing Epoxy Matrix, M35-4/40%/G1089/1000 Fabric Fiber: T800H 6K 2x2 Twill, 200 g/m2Information provided by HexCel |