Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 8.83 MPa @Temperature 23.0 °C |
1280 psi @Temperature 73.4 °F |
Overlap, Polyacrylic, Substrate Failure |
3M Scotch-Weld™ TS230 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |
|||
Shear Strength | 8.83 MPa @Temperature 23.0 °C |
1280 psi @Temperature 73.4 °F |
Overlap, Polyacrylic, Substrate Failure |
3M Scotch-Weld™ EZ250150 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds a wide variety of plastics and wood to th.. |
|||
Shear Strength | 8.83 MPa @Time 86400 sec |
1280 psi @Time 24.0 hour |
Overlap, Maple |
3M Scotch-Weld™ EZ250150 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds a wide variety of plastics and wood to th.. |