Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 13.4 MPa @Temperature 23.0 °C |
1950 psi @Temperature 73.4 °F |
Overlap, Maple |
3M Scotch-Weld™ EZ250120 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds well to wood and wood bases surfaces as w.. |
|||
Shear Strength | 13.4 MPa @Time 605000 sec |
1950 psi @Time 168 hour |
Overlap, Maple conditioned for 7 days AT RT/50% RH |
3M Scotch-Weld™ EZ250120 Polyurethane Reactive (PUR) Easy 250 Wood Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive (PUR) Easy 250 Wood Adhesive is 100% solid, warm temperature applied, moisture curing urethanes. This product bonds well to wood and wood bases surfaces as w.. |
|||
Shear Strength | 13.4 MPa @Temperature 23.0 °C |
1950 psi @Temperature 73.4 °F |
Overlap, Maple |
3M Scotch-Weld™ TE200 Polyurethane Reactive Adhesive 3M™ Scotch-Weld™ Polyurethane Reactive Adhesives are a family of one-component, moisture curing, urethane adhesives. These adhesives are applied warm and bond a wide variety of substrates such as .. |