Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 91.7 MPa @Temperature 121 °C |
13300 psi @Temperature 250 °F |
In-Plane, Dry; 270°F Oven Cure, 350°F Postcure; ASTM D3518 |
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, 6K 5HS T300 Reinforced Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois.. |
|||
Shear Strength | 92.0 MPa @Temperature 23.0 °C |
13300 psi @Temperature 73.4 °F |
0º Interlaminar Shear, Conditioning: 23°C; ASTM D2344 |
Hexcel® HexPly® M47 140°C Curing Epoxy Matrix, Unidirectional Carbon Prepreg IM2-C Fibre 1947 - 38% resin weight with IM2-C 53% fiber volumeInformation provided by HexCel |