Material Notes:
Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good moisture resistance, as well as excellent tack and drape. Formulated for both oven and autoclave cure, E-752 provides for easy processing with oven cure, without sacrificing mechanical properties.Key Features and Benefits:Specifically designed to allow both oven cure and autoclave cureAllows oven curing without sacrificing mechanical propertiesService temperatures up to 130°CControlled flow for ease of processingFlexible cure temperature 132°C to 185°CGood mechanical properties can be achieved through oven curing at 132°C, followed by post-cure at 185°CSelf-adhesive grade for sandwich panel applicationsApplications/Qualifications:Primary and Secondary Aircraft StructuresDuctingFairingsNacellesInformation provided by Park Electrochemical Corp.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 820 MPa

@Temperature 23.9 °C
119000 psi

@Temperature 75.0 °F
0° Direction; 270°F Oven Cure, 350°F Postcure; ASTM D3039
820 MPa

@Temperature 121 °C
119000 psi

@Temperature 250 °F
0° Direction; 270°F Oven Cure, 350°F Postcure; ASTM D3039
827 MPa

@Temperature 121 °C
120000 psi

@Temperature 250 °F
0° Direction; 270°F Oven Cure, 350°F Postcure; ASTM D3039
Tensile Modulus 65.5 GPa

@Temperature 121 °C
9500 ksi

@Temperature 250 °F
0° Direction; 270°F Oven Cure, 350°F Postcure; ASTM D3039
65.5 GPa

@Temperature 121 °C
9500 ksi

@Temperature 250 °F
0° Direction; 270°F Oven Cure, 350°F Postcure; ASTM D3039
66.2 GPa

@Temperature 23.9 °C
9600 ksi

@Temperature 75.0 °F
0° Direction; 270°F Oven Cure, 350°F Postcure; ASTM D3039
Compressive Strength 319 MPa

@Temperature 23.9 °C
46300 psi

@Temperature 75.0 °F
Open-Hole, Dry; 270°F Oven Cure, 350°F Postcure; ASTM D6484
607 MPa

@Temperature 121 °C
88000 psi

@Temperature 250 °F
Wet; 270°F Oven Cure, 350°F Postcure; SACMA 1R-94
717 MPa

@Temperature 121 °C
104000 psi

@Temperature 250 °F
Dry; 270°F Oven Cure, 350°F Postcure; SACMA 1R-94
827 MPa

@Temperature 23.9 °C
120000 psi

@Temperature 75.0 °F
Dry; 270°F Oven Cure, 350°F Postcure; SACMA 1R-94
Compressive Modulus 44.8 GPa

@Temperature 23.9 °C
6500 ksi

@Temperature 75.0 °F
Open-Hole, Dry; 270°F Oven Cure, 350°F Postcure; ASTM D6484
60.0 GPa

@Temperature 121 °C
8700 ksi

@Temperature 250 °F
Wet; 270°F Oven Cure, 350°F Postcure; SACMA 1R-94
61.4 GPa

@Temperature 23.9 °C
8900 ksi

@Temperature 75.0 °F
Dry; 270°F Oven Cure, 350°F Postcure; SACMA 1R-94
61.4 GPa

@Temperature 121 °C
8900 ksi

@Temperature 250 °F
Dry; 270°F Oven Cure, 350°F Postcure; SACMA 1R-94
Shear Modulus 4.69 GPa

@Temperature 121 °C
680 ksi

@Temperature 250 °F
In-Plane, Wet; 270°F Oven Cure, 350°F Postcure; ASTM D3518
4.76 GPa

@Temperature 23.9 °C
690 ksi

@Temperature 75.0 °F
In-Plane, Dry; 270°F Oven Cure, 350°F Postcure; ASTM D3518
4.83 GPa

@Temperature 121 °C
700 ksi

@Temperature 250 °F
In-Plane, Dry; 270°F Oven Cure, 350°F Postcure; ASTM D3518
Shear Strength 79.3 MPa

@Temperature 121 °C
11500 psi

@Temperature 250 °F
In-Plane, Wet; 270°F Oven Cure, 350°F Postcure; ASTM D3518
91.7 MPa

@Temperature 121 °C
13300 psi

@Temperature 250 °F
In-Plane, Dry; 270°F Oven Cure, 350°F Postcure; ASTM D3518
97.2 MPa

@Temperature 23.9 °C
14100 psi

@Temperature 75.0 °F
In-Plane, Dry; 270°F Oven Cure, 350°F Postcure; ASTM D3518
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature -17.8 °C
12.0 Month

@Temperature 0.000 °F
Descriptive Properties Value Comments
Fabric Area Weight (g/m²) 378
270°F Oven Cure, 350°F Postcure