Mechanical Properties Metric English Comments
Shear Strength 99.0 MPa

@Temperature 22.0 °C
14400 psi

@Temperature 71.6 °F
0°, IL
Hexcel® HexPly® 954-6 Curing Cyanate Resin, M40J Fiber
Information provided by HexCel