Shear Strength 15.5 MPa

@Temperature 93.3 °C
2250 psi

@Temperature 200 °F
ASTM D732
Greene Tweed Avalon® 9 PTFE, Graphite Filled
Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin..
Shear Strength 15.5 MPa

@Temperature 22.0 °C
2250 psi

@Temperature 71.6 °F
Tube Shear; Dry; 30 min @ 150°C; EN2667-2
Hexcel® Redux® 840 One-part Foaming Epoxy Paste Adhesive
Redux® 840 is a black one-part, foaming, epoxy paste adhesive that is thixotropic.Features: Provides a shear-carrying connection across any discontinuities in bonded sandwich panels; Maximum servic..
Shear Strength 15.5 MPa

@Temperature 22.0 °C
2250 psi

@Temperature 71.6 °F
Double Lap Shear; Dry; 30 min @ 150°C; Hexcel IS202
Hexcel® Redux® 840 One-part Foaming Epoxy Paste Adhesive
Redux® 840 is a black one-part, foaming, epoxy paste adhesive that is thixotropic.Features: Provides a shear-carrying connection across any discontinuities in bonded sandwich panels; Maximum servic..
Shear Strength 15.5 MPa

@Temperature 23.0 °C
2250 psi

@Temperature 73.4 °F
Overlap, FRP
3M Scotch-Weld™ TS230 Polyurethane Reactive Adhesive