Material Notes:
Products made from Avalon® thermoplastics are constructed from proprietary high-performance reinforced PTFE material. Greene, Tweeds Avalon thermoplastics, available in grades ranging from virgin to reinforced, exhibit low friction while being chemically inert. Avalon thermoplastics can be custom designed to for each unique application.Information provided by Greene Tweed.
Physical Properties Metric English Comments
Specific Gravity 2.12 g/cc
2.12 g/cc
ASTM D792
Deformation 8.0 %
8.0 %
2000 psi 78°F; ASTM D621
14 %
14 %
1000 psi 300°F; ASTM D621
Mechanical Properties Metric English Comments
Hardness, Shore D 55
55
ASTM D2240
Tensile Strength, Yield 17.9 MPa
2600 psi
ASTM D1457
Elongation at Break 225 %
225 %
ASTM D1457
Compressive Strength 23.4 MPa
3400 psi
ASTM D695
Shear Strength 14.5 MPa

@Temperature 149 °C
2100 psi

@Temperature 300 °F
ASTM D732
15.5 MPa

@Temperature 93.3 °C
2250 psi

@Temperature 200 °F
ASTM D732
16.5 MPa

@Temperature 65.6 °C
2400 psi

@Temperature 150 °F
ASTM D732
18.6 MPa

@Temperature 37.8 °C
2700 psi

@Temperature 100 °F
ASTM D732
19.3 MPa

@Temperature 26.7 °C
2800 psi

@Temperature 80.0 °F
ASTM D732
Coefficient of Friction, Dynamic 0.070
0.070
33.3 psi @ 150 fpm
Coefficient of Friction, Static 0.050
0.050
33.3 psi
K (wear) Factor 60.4 x 10-8 mm³/N-M
30.0 x 10-10 in³-min/ft-lb-hr
Descriptive Properties Value Comments
Color Dark Gray to Black