Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 118 MPa @Temperature 23.0 °C |
17100 psi @Temperature 73.4 °F |
Short Beam; [0°]; Resin Content=29%, Fiber Volume=64% |
Hexcel® HexPly® F650 Bismaleimide Resin with IM6 Fiber Composition: IM6 Fiber, 12K, G sizes, UD Tape - 145 g/m2Information provided by HexCel |
|||
Shear Strength | 118 MPa @Temperature 23.0 °C |
17100 psi @Temperature 73.4 °F |
In-Plane; prEN6032 |
Hexcel® HexPly® M35-4 80-180°C Curing Epoxy Matrix, M35-4/40%/48280/1000 Fabric Fiber: T1000 12K 5H Satin, 283 g/m2Information provided by HexCel |