Mechanical Properties Metric English Comments
Shear Strength 23.8 MPa

@Temperature -55.0 °C
3450 psi

@Temperature -67.0 °F
Tensile Lap Shear; Aluminum Primer HP655P; ASTM D1002
Hexcel® Redux® HP655 Toughened BMI film Adhesive
Redux® HP655 is a toughened BMI structural adhesive designed for metal to metal, composite to composite, and honeycomb sandwich bonding for both co-cured and precured composite skins. Redux® HP655..