Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 24.0 MPa @Temperature 23.9 °C |
3480 psi @Temperature 75.0 °F |
Cure cycle: 7 days @ RT (+7 days water soak), with Aced Etched 6061-T6 Aluminum |
Zyvex Performance Materials Epovex™ Nano-Engineered Composite Epoxy Adhesive Liquid Epovex® Adhesive is a carbon nanotube enhanced ambient or elevated temperature cure two-part epoxy adhesive. Used for bonding, laminating, filling or potting, Epovex is ideal for many metals, woods.. |
|||
Shear Strength | 24.0 MPa @Temperature 50.0 °C |
3480 psi @Temperature 122 °F |
Lap Shear |
Hexcel® Redux® 610W (0.06 psf) Flame retarded epoxy film adhesive Redux 610 is a modified, flame-retarded epoxy film adhesive curing at 250°F. It is suitable for bonding metal to metal and for sandwich structures where flame retardancy and low heat release are re.. |
|||
Shear Strength | 24.0 MPa @Temperature 1000 °C |
3480 psi @Temperature 1830 °F |
|
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon Engineered ceramic composite structure.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiCPhysical Attributes: Dense Matrix ( |