Polymer Property : Shear Strength = 39.3 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Shear Strength 39.3 MPa

@Temperature 82.2 °C
5700 psi

@Temperature 180 °F
Short-Beam, Wet; Vacuum/Oven Cured; ASTM D2344
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T700 Uni Tape Reinforced
Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request...
Shear Strength 39.3 MPa

@Temperature 71.1 °C
5700 psi

@Temperature 160 °F
Lap Shear
Hexcel® Redux® 312 Modified epoxy film adhesive (0.06 psf)
Redux® 312 is a high-strength 250°F curing film adhesive, suitable for metal to metal bonding and sandwich constructions, where operating temperatures of up to 210°F may be experienced. A support..
Shear Strength 39.3 MPa

@Temperature 21.1 °C
5700 psi

@Temperature 70.0 °F
Lap Shear
Hexcel® Redux® 312UL Modified epoxy film adhesive
Redux® 312 is a high-strength 250°F curing film adhesive, suitable for metal to metal bonding and sandwich constructions, where operating temperatures of up to 210°F may be experienced. A support..
Shear Strength 39.3 MPa

@Temperature 21.1 °C
5700 psi

@Temperature 70.0 °F
Lap Shear
Hexcel® Redux® 335K Adhesive film for bonding metallic and composite components (0.06 psf)
Redux 335 is a film adhesive curing at 250F. It is available in a range of standard areal weights from 0.015 to 0.06 psf. It is available either unsupported or with knitted and/or matt carrier for a..