Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Shear Strength | 39.3 MPa @Temperature 82.2 °C |
5700 psi @Temperature 180 °F |
Short-Beam, Wet; Vacuum/Oven Cured; ASTM D2344 |
Park Electrochemical Nelcote® E-765 Epoxy Prepreg, T700 Uni Tape Reinforced Nelcote® E-765 is a tough 250°F cure prepreg system designed to replace 350°F cure systems in aircraft structural applications. FAA-approved Design Allowable Databases are available upon request... |
|||
Shear Strength | 39.3 MPa @Temperature 71.1 °C |
5700 psi @Temperature 160 °F |
Lap Shear |
Hexcel® Redux® 312 Modified epoxy film adhesive (0.06 psf) Redux® 312 is a high-strength 250°F curing film adhesive, suitable for metal to metal bonding and sandwich constructions, where operating temperatures of up to 210°F may be experienced. A support.. |
|||
Shear Strength | 39.3 MPa @Temperature 21.1 °C |
5700 psi @Temperature 70.0 °F |
Lap Shear |
Hexcel® Redux® 312UL Modified epoxy film adhesive Redux® 312 is a high-strength 250°F curing film adhesive, suitable for metal to metal bonding and sandwich constructions, where operating temperatures of up to 210°F may be experienced. A support.. |
|||
Shear Strength | 39.3 MPa @Temperature 21.1 °C |
5700 psi @Temperature 70.0 °F |
Lap Shear |
Hexcel® Redux® 335K Adhesive film for bonding metallic and composite components (0.06 psf) Redux 335 is a film adhesive curing at 250F. It is available in a range of standard areal weights from 0.015 to 0.06 psf. It is available either unsupported or with knitted and/or matt carrier for a.. |